PRODUCT |
DESCRIPTION |
ADVANTAGES |
| RETARDERS |
| FR-1/FR-1L |
A Lignosulfonate, <250ºF |
Economical retarder |
| FR-2/FR-2L |
A Non-Lignosulfonate polymer, <250ºF |
Saves rig time by better control of pumping time and more rapid strength development especially at
top of cement |
| PCR-2/PCR-2L |
Acrylic Terpolymer, <250°F, salt <350°F |
| PCR-3/PCR-3L |
Acrylic Terpolymer, <250°F, salt <350°F |
| PCR-4/PCR-4L |
Retarder Intensifier, <430°F |
Used to increase thickening times at elevated temperature |
| ACCELERATORS |
| FL-7/FL-7L |
Cellulose/dispersant, Fresh water, low salt, <250°F |
Low temperature and economical |
| DISPERSANTS |
| NC-S-1/NC-S-1L |
Sulfonated polymer, Freshwater, low salt |
Provides a lower viscosity slurry for
lower frictional pressure. Can be
used for densification |
| SC-8/SC-8L |
Sulfonated polymer, Freshwater, Saltwater |
| SC-9/SC-9L |
Sulfonated polymer, Freshwater, Saltwater |
| FLUID LOSS ADDITIVES |
| FL-7/FL-7L |
Cellulose/dispersant, Fresh water, low salt,<250°F |
Low temperature and economical |
| FL-14/FL-14L |
Polymer, Fresh water, low salt, 80-350°F |
Provides low gel strength and mild
retardation. Can be used in low
density and high-density slurries.
FL-17 can be considered universal
for all cementing. FL-14 and FL- 17
are especially good for squeeze
cementing because of low gel
strength. |
| FL-17/FL-17L |
Polymer, Fresh water, saltwater, 80-400°F |
| GAS MIGRATION |
| FL-14/FL-14L |
Polymer, Fresh water, low salt, 80-350°F |
Low gel strength and short
transition times |
| FL-17/FL-17L |
Polymer, Fresh water, saltwater, 80-400°F |
| DEFOAMERS |
| DEFOAMER 7011/7011L |
Decrease foaming and air entrainment |
Provides an accurate measurement
of slurry density during mixing |
| DEFOAMER 3022L |
Defoamer for latexes, surfactants and liquidadditives in the mix water |
| DEFOAMER 7500L |
Decrease foaming and air entrainment |
Economical defoamer |
| CEMENT SPACER |
| EZ-SPACER One |
One sack system, just add water and barite, <350°F |
Provides for easy shipping, handling
on location and easy mixing to
achieve desired density |
| THIXOTROPIC ADDITIVES |
| THIXAD I |
Low temperature lost circulation |
Imparts very short transition time to
the cement slurry for shallow loss
circulation and gas migration |
| THIXAD 2 |
Low temperature lost circulation |
| FREE WATER CONTROL |
| HTSA-1 |
Controls free water at temperature >200°F; no increase in mixing viscosity |
Allows control of free water and
prevents separation of solids at
elevated temperature |
| SPECIALTY |
| PUMP FLUSH PLUS |
A solvent system for cleaning oil and diesel |
Cleans additive pumps and lines for removal of water ahead of mineral oil and diesel suspension products. Also cleans after the job |
| FLY ASH (CLASS C) |
Bagged |
Light weight cement systems |
#1 SILICA SAND
(100 MESH) |
Bagged, Strength stabilizer >230°F |
Prevents cement compressive
strength retrogression and
increased permeability at elevated
temperature |
SILICA FLOUR
(200 MESH ) |
Bagged, Strength stabilizer >230°F |
SILICA FLOUR
(270 MESH ) |
Bagged, Strength stabilizer >230°F |